Seismic cracking from U/S and D/S faces
CADAM3D allows cracking to initiate either from the u/s face or the d/s face depending upon the orientation of the base acceleration and related inertia forces. Separate analyses could be performed successively with the base acceleration pointing u/s and d/s to estimate the cumulative damage reducing the cohesion that could be mobilised along the joint considered.